Applications of two electric arc plasma torches for the beneficiation of natural quartz
Yuri-Mikhailovich Grishin, Long Miao, Lev-Alekseevich Borisov, Nikolay-Mikhailovich Serykh, Alexey-Yurievich Kulagin
2019, 26(3): 267-273. DOI: 10.1007/s12613-019-1734-8
中文摘要 PDF SpringerLink
Accelerating leaching of copper ore with surfactant and the analysis of reaction kinetics
Chun-ming Ai, Ping-ping Sun, Ai-xiang Wu, Xun Chen, Chao Liu
2019, 26(3): 274-281. DOI: 10.1007/s12613-019-1735-7
中文摘要 PDF SpringerLink
Austenite grain growth of medium-carbon alloy steel with aluminum additions during heating process
Zi-yi Liu, Yan-ping Bao, Min Wang, Xin Li, Fan-zheng Zeng
2019, 26(3): 282-290. DOI: 10.1007/s12613-019-1736-6
中文摘要 PDF SpringerLink
Effect of slag on oxide inclusions in carburized bearing steel during industrial electroslag remelting
Shi-jian Li, Guo-guang Cheng, Zhi-qi Miao, Lie Chen, Xin-yan Jiang
2019, 26(3): 291-300. DOI: 10.1007/s12613-019-1737-5
中文摘要 PDF SpringerLink
Relationship between copper content of slag and matte in the SKS copper smelting process
Qin-meng Wang, Song-song Wang, Miao Tian, Ding-xuan Tang, Qing-hua Tian, Xue-yi Guo
2019, 26(3): 301-308. DOI: 10.1007/s12613-019-1738-4
中文摘要 PDF SpringerLink
Feasibility of aluminum recovery and MgAl2O4 spinel synthesis from secondary aluminum dross
Yong Zhang, Zhao-hui Guo, Zi-yu Han, Xi-yuan Xiao, Chi Peng
2019, 26(3): 309-318. DOI: 10.1007/s12613-019-1739-3
中文摘要 PDF SpringerLink
Anisotropy in mechanical properties and corrosion resistance of 316L stainless steel fabricated by selective laser melting
Xiao-qing Ni, De-cheng Kong, Ying Wen, Liang Zhang, Wen-heng Wu, Bei-bei He, Lin Lu, De-xiang Zhu
2019, 26(3): 319-328. DOI: 10.1007/s12613-019-1740-x
中文摘要 PDF SpringerLink
Passivity breakdown of 13Cr stainless steel under high chloride and CO2 environment
Hui-xin Li, Da-peng Li, Lei Zhang, Ya-wen Wang, Xiu-yun Wang, Min-xu Lu
2019, 26(3): 329-336. DOI: 10.1007/s12613-019-1741-9
中文摘要 PDF SpringerLink
Hot-corrosion behavior of Cr2O3-CNT-coated ASTM-SA213-T22 steel in a molten salt environment at 700℃
Khushdeep Goyal, Hazoor Singh, Rakesh Bhatia
2019, 26(3): 337-344. DOI: 10.1007/s12613-019-1742-8
中文摘要 PDF SpringerLink
Synthesis of a NiTi2-AlNi-Al2O3 nanocomposite by mechanical alloying and heat treatment of Al-TiO2-NiO
Reza Beygi, Majid Zarezadeh Mehrizi, Hossein Mostaan, Mahdi Rafiei, Ahmadreza Abbasian
2019, 26(3): 345-349. DOI: 10.1007/s12613-019-1743-7
中文摘要 PDF SpringerLink
Carbon deposition in porous nickel/yttria-stabilized zirconia anode under methane atmosphere
Zhi-yuan Chen, Li-jun Wang, Xiao-jia Du, Zai-hong Sun, Fu-shen Li, Kuo-Chih Chou
2019, 26(3): 350-359. DOI: 10.1007/s12613-019-1744-6
中文摘要 PDF SpringerLink
Enhanced elevated temperature wear resistance of Al-17Si-5Cu alloy after a novel short duration heat treatment
Biplab Hazra, Supriya Bera, Bijay Kumar Show
2019, 26(3): 360-368. DOI: 10.1007/s12613-019-1745-5
中文摘要 PDF SpringerLink
Microstructure and finite element analysis of hot continuous rolling of doped tungsten rod
Zheng-jie Shao, Hai-po Liu, Xiao-chun He, Bing Zhou, Yang Li, Shang-zhou Zhang, Meng-jin Li, Shu-jun Li
2019, 26(3): 369-376. DOI: 10.1007/s12613-019-1746-4
中文摘要 PDF SpringerLink
Numerical simulation and experimental verification of a novel double-layered split die for high-pressure apparatus used for synthesizing superhard materials
Zhuo Yi, Wen-zhi Fu, Ming-zhe Li, Rui Li, Liang Zhao, Li-yan Wang
2019, 26(3): 377-385. DOI: 10.1007/s12613-019-1747-3
中文摘要 PDF SpringerLink
Erratum to: Lithium-ion full cell with high energy density using nickel-rich LiNi0.8Co0.1Mn0.1O2 cathode and SiO-C composite anode
Azhar Iqbal, Long Chen, Yong Chen, Yu-xian Gao, Fang Chen, Dao-cong Li
2019, 26(3): 386-386. DOI: 10.1007/s12613-019-1732-x
中文摘要 PDF SpringerLink